Construction and storage of epoxy resin anti-corrosion steel pipe

(1) The dust, oil, oxide scale, etc. on the surface of the object must be cleaned before painting. Reach Sa 2.5 to guarantee the quality of the painting. It is strictly forbidden to bring water into the construction.

(2) The construction proportioning method is as follows: open the mouth of component A, add component B into component A, and stir well. After curing for 30 minutes, it can be painted.
(3) This material is required to be used as needed, and the mixed paint must be used up within eight hours. Unfinished materials should be sealed and stored. Construction should be stopped on cloudy and rainy days or when the relative temperature is greater than 75%. For the parts with severe corrosive medium, it is recommended to apply multiple coats.
(4) The product should be stored in a cool and dry place, prevent direct sunlight, isolate the fire source, and keep away from the heat source. The storage period is 12 months. After the expiration, all technical indicators should be inspected. If the requirements of the indicators are met, they can continue to be used.
Back

Related Information

Construction and storage of epoxy resin anti-corrosion steel pipe

Copyright © 2017-2021 Threeway Steel CO., LTD. All rights reserved.    Sitemap 

Other friends: Threewaysteel, Threeway-pipe