Welcome to http://www.srtsteelpipe.com
   
ASTM A179 Seamless Steel Pipe - Threeway Steel Co.,Ltd
BackHome - Product > Seamless Steel Pipe > Carbon Steel Pipe
ASTM A179, ASTM A192,  ASTM A210
  • ASTM A179, ASTM A192,  ASTM A210

ASTM A179, ASTM A192, ASTM A210

Standard:
American society of mechanical engineers ASME SA 179,ASME SA 192,ASME
SA 210; American society for Testing and Materials ASTM A179M,ASTM A192M,ASTM A210M
Uses: For manufacture wall panel, economizer, reheater, superheater and steam pipeline of boilers.

...

Inquiry

  • Description
  • Size

ASTM A179 Seamless Steel Pipe:

Chemical Composition(%): 


Grade

C

Si

Mn

S

P

Standard

Steel grade

Max

ASTM

A 192        SA-192

0.06-0.18

=

0.27-0.63

0.02

0.025

A 192M

0.025

ASME

SA-192M

ASTM

A 179        SA 179

0.06-0.18

-

0.27-0.63

0.035

0.035

A 179

ASME

SA-179

ASTM

A 210A1

=

=

=

0.02

0.025

A 210M

SA-210A1

0.27

0.1

0.93

ASME

A 210C

=

=0.10

0.29-1.06

0.02

0.025

SA-210M

SA-210C

0.35




Mechanical Properties: 


Standard

Grade

Tensile strength

Yield strength (MPa)

Elongation (%)

Impact (J)

Hardness

not less than

not less than

not less than

not less than

ASTMA 192M ASME SA-192M

A 192/SA-192

=325

180

35

-

77HRB(137HBW)

ASME SA179 ASTM A179

SA 179/A 179

=325

180

35

-

 ASTMA 210M ASME SA-210M

A210A1/SA-210A1

=415

255

-

79HRB(143HBW)

A210C/SA-210C

=485

275

-

89HRB(179HBW)



American society of mechanical engineers: ASME SA-106, ASME SA-192M, ASME SA-209M, ASME SA-210M, ASME SA-213M, ASME SA-335M, ASME SA-179M

American Society for Testing and Materials : ASTM A 106M, ASTM A 192M, ASTM A 210M, ASTM A 213M, ASTM A 335M, ASTM A 179M

European Standards: EN 10216-2

Deutsches Institut fur Normung: DIN 17175

Japaneses industrial standards: JIS G 3456, JIS G 3461, JIS G 3462

Uses: For manufacture wall panel, economizer, reheater6 superheater and steam pipeline of boilers


ASTM A179 Seamless Steel Pipe:

Chemical Composition(%): 


Grade

C

Si

Mn

S

P

Standard

Steel grade

Max

ASTM

A 192        SA-192

0.06-0.18

=

0.27-0.63

0.02

0.025

A 192M

0.025

ASME

SA-192M

ASTM

A 179        SA 179

0.06-0.18

-

0.27-0.63

0.035

0.035

A 179

ASME

SA-179

ASTM

A 210A1

=

=

=

0.02

0.025

A 210M

SA-210A1

0.27

0.1

0.93

ASME

A 210C

=

=0.10

0.29-1.06

0.02

0.025

SA-210M

SA-210C

0.35




Mechanical Properties: 


Standard

Grade

Tensile strength

Yield strength (MPa)

Elongation (%)

Impact (J)

Hardness

not less than

not less than

not less than

not less than

ASTMA 192M ASME SA-192M

A 192/SA-192

=325

180

35

-

77HRB(137HBW)

ASME SA179 ASTM A179

SA 179/A 179

=325

180

35

-

 ASTMA 210M ASME SA-210M

A210A1/SA-210A1

=415

255

-

79HRB(143HBW)

A210C/SA-210C

=485

275

-

89HRB(179HBW)



American society of mechanical engineers: ASME SA-106, ASME SA-192M, ASME SA-209M, ASME SA-210M, ASME SA-213M, ASME SA-335M, ASME SA-179M

American Society for Testing and Materials : ASTM A 106M, ASTM A 192M, ASTM A 210M, ASTM A 213M, ASTM A 335M, ASTM A 179M

European Standards: EN 10216-2

Deutsches Institut fur Normung: DIN 17175

Japaneses industrial standards: JIS G 3456, JIS G 3461, JIS G 3462

Uses: For manufacture wall panel, economizer, reheater6 superheater and steam pipeline of boilers