Austenitic stainless stee l: Austenitic stainless steel generally belongs to corrosion-resistant steel and is the most widely used type of steel. Among them, 18-8 stainless steel is the most representative. It has good mechanical properties and is convenient for machining, stamping, and welding. ...
Keywords :What will happen to the stainless steel pipe after pickling Update : 2023-03-06 View(s) : 649
With the wide application of stainless steel pipes , people's requirements for them are getting higher and higher, and the processing technology has become diversified. Pickling is one of the processing techniques. Do you know why hydrogen embrittlement occurs in stainless steel pipes after pickl...
Keywords :Anti-corrosion measures for long-distance natural gas steel pipelines Update : 2023-03-03 View(s) : 587
In the actual steel pipeline transportation process, in essence, steel pipeline corrosion is a normal phenomenon and cannot be completely avoided. Reducing the impact of pipeline corrosion on natural gas transportation can only be alleviated through the application of corresponding measures, to ...
Keywords :How to cool the large diameter steel pipe after the quenching process Update : 2023-03-02 View(s) : 600
(1) During the quenching process, the workpiece must be heated to a higher temperature and cooled at a faster rate. Therefore, during quenching, especially during the quenching and cooling process, a large thermal stress will be generated. When a steel ball with a diameter of 26 mm is cooled in wate...
Keywords :Pre-welding and welding of straight seam steel pipe Update : 2023-03-01 View(s) : 574
Pre-welding of straight seam steel pipes : pre-welding includes seams and welds. 1. The joint (that is, the forming seam) has no misalignment or the misalignment is less than the specified value. Generally, the amount of misalignment is ≤ 8% of the plate thickness, and the maximum is not more t...